logo-3D-print-it

Properties:

  • easy feeding of filament to the extruder – the material does not break
  • possibility of grinding, polishing, varnishing and colouring the prints

How to print?

  • print temperature: 190-210°C (374-410°F)
  • bed temperature: 50-70°C (122-158°F) (when using plates or other means to increase the adhesion, the heating of the bed is not required)
  • to avoid a situation where the nozzle gets clogged with wood particles, we recommend cleaning the extruder after each FiberWood print by using any type of PLA filament
  • suggested min. diameter tolerance – 0,5 mm
  • 0.75kg rol
  • 1.75mm

Wood Filament Bruin

 36,00

(Incl. 21% BTW – Exclusief verzendkosten)

Beschikbaar via nabestelling