- biodegradability
- slightly glossy surface
- possibility of annealing the print in an oven and achieving properties similar to those of ABS
- after annealing – increased impact resistance and high temperature resistance
How to print?
- print temperature: 200-220°C
- bed temperature: 50-70°C (when using plates or other means to increase the adhesion, the heating of the bed is not required)
- heating of the print should be conducted in accordance with the manual provided by Fiberlogy
- 0.85kg rol
- 1.75mm